Analisis Pengaruh Bahan PIN terhadap Sifat Mekanik dan Struktur Mikro Sambungan Plat Aluminium pada Proses Friction Stir Welding

Mahendra, Ricky Oka and , Ir. Bibit Sugito, MT (2019) Analisis Pengaruh Bahan PIN terhadap Sifat Mekanik dan Struktur Mikro Sambungan Plat Aluminium pada Proses Friction Stir Welding. Skripsi thesis, Universitas Muhammadiyah Surakarta.

[img] PDF (Naskah Publikasi)
Naskah Publikasi-124.pdf

Download (1MB)
[img] PDF (Halaman Depan)
Halaman Depan-109.pdf

Download (1MB)
[img] PDF (Bab I)
BAB I.pdf

Download (38kB)
[img] PDF (Bab II)
BAB II.pdf
Restricted to Repository staff only

Download (383kB) | Request a copy
[img] PDF (Bab III)
BAB III .pdf
Restricted to Repository staff only

Download (870kB) | Request a copy
[img] PDF (Bab IV)
BAB IV.pdf
Restricted to Repository staff only

Download (665kB) | Request a copy
[img] PDF (Bab V)
BAB V.pdf
Restricted to Repository staff only

Download (34kB) | Request a copy
[img] PDF (Daftar Pustaka)
DAFTAR PUSTAKA.pdf

Download (18kB)
[img] PDF (Lampiran)
Lampiran.pdf
Restricted to Repository staff only

Download (2MB) | Request a copy
[img] PDF (Pernyataan Publikasi Ilmiah)
Pernyataan publikasi ilmiah.pdf
Restricted to Repository staff only

Download (607kB) | Request a copy

Abstract

Aluminum material (Al) and both have been widely used in the industrial sector. Welding in this study uses aluminum material and welding using friction stir welding. Twisted friction welding technology is a potential alternative to be applied to aluminum. This study aims to determine the mechanical properties and microstructure of aluminum plate joints in the friction stir welding process. with a variety of pin material. In this welding study the parameters used are the rotational speed of 2280rpm, feed speed of 60 mm / minute. The pin material uses AISI 4340 steel, AISI O1 and AISI D2. In this study, the X8140A model of the brand Richon vertical freis machine was used and the connection using a butt joint, by looking at the analysis of the strength of the weld results compared to other welding. The results of this test show that the maximum welding tensile stress using the AISI 4340 tool joint is 78.01 Mpa and the maximum strain using the AISI D2 tool joint is 22.51%. Hardness testing in the stir zone area all experienced an increase in hardness value compared to base metal and HAZ regions. Microstructure testing on the stir zone area showed smaller and finer grain sizes compared to the HAZ and base metal regions, so that the stir zone area had a higher hardness value than the HAZ and base metal regions.

Item Type: Karya ilmiah (Skripsi)
Uncontrolled Keywords: FSW, Bahan Pin, Sifat Mekanik, Struktur Mikro
Subjects: T Technology > T Technology (General)
Divisions: Fakultas Teknik > Teknik Mesin
Depositing User: RICKY OKA MAHENDRA
Date Deposited: 03 Sep 2019 03:33
Last Modified: 03 Sep 2019 03:33
URI: http://eprints.ums.ac.id/id/eprint/77590

Actions (login required)

View Item View Item