Juliarto, Alwan and , Ir. Bibit Sugito, MT (2019) Analisa Pengaruh Perlakuan Panas Hasil Pengelasan dengan Metode Friction Stir Welding (FSW) pada AA-7075 terhadap Sifat Fisis dan Mekanis. Skripsi thesis, Universitas Muhammadiyah Surakarta.
PDF (Naskah Publikasi)
NASKAH PUBLIKASI-1.pdf Download (971kB) |
|
PDF (Halaman Depan)
HALAMAN DEPAN-7.pdf Download (1MB) |
|
PDF (Bab I)
BAB I .pdf Download (248kB) |
|
PDF (Bab II)
BAB II .pdf Restricted to Repository staff only Download (603kB) | Request a copy |
|
PDF (Bab III)
BAB III .pdf Restricted to Repository staff only Download (427kB) | Request a copy |
|
PDF (Bab IV)
BAB IV .pdf Restricted to Repository staff only Download (724kB) | Request a copy |
|
PDF (Bab V)
BAB V .pdf Restricted to Repository staff only Download (11kB) | Request a copy |
|
PDF (Daftar Pustaka)
DAFTAR PUSTAKA.pdf Download (11kB) |
|
PDF (Lampiran)
LAMPIRAN.pdf Restricted to Repository staff only Download (2MB) | Request a copy |
|
PDF (Pernyataan Publikasi Ilmiah)
SURAT PERNYATAAN.pdf Restricted to Repository staff only Download (201kB) | Request a copy |
Abstract
Friction Stir Welding (FSW) is a welding process utilizing heat due to rotation of the tool that rubs against the parent metal under large axial pressure in the welding area. This study aims to know changes in physical and mechanical properties of Friction Stir Welding (FSW) followed by heat treatment of annealing and normalizing.The FSW process uses a milling machine. The material used is AA-7075 with a size of 150×50×30 mm, tool rotation 1500 rpm, tool tilt angle 3˚ and feed rate 60 mm / minute with the type of butt joint welding joint. Annealing and normalizing treatments were carried out at 415˚C for 2 hours of heat retention in the furnace. Specimen testing includes, tensile test, hardness test, and microstructure photo.From the results of the study it was found that the highest tensile strength in raw material with an average stress and strain value of 218.2 Mpa and 12.6%, the highest hardness value of base metal in raw material was 80.90 BHN, HAZ area and weld the highest hardness value in material experiencing normalizing is equal to 57.97 BHN and 69.47 BHN. From the observation of the micro structure there is a bright area which is the Al phase and the dark region which is the MgZn2 phase.
Item Type: | Karya ilmiah (Skripsi) |
---|---|
Uncontrolled Keywords: | FSW, AA-7075, heat treatment, annealing, normalizing |
Subjects: | T Technology > TJ Mechanical engineering and machinery T Technology > TS Manufactures |
Divisions: | Fakultas Teknik > Teknik Mesin |
Depositing User: | ALWAN JULIARTO |
Date Deposited: | 29 Jan 2019 01:48 |
Last Modified: | 29 Jan 2019 01:48 |
URI: | http://eprints.ums.ac.id/id/eprint/70163 |
Actions (login required)
View Item |