Yanto, Danang Dany and , Tri widodo Besar Riyadi, ST, M.Sc, Ph.D (2018) Pengaruh Elektroplating Nikel Terhadap Ketebalan Lapisan, Kekasaran, dan Kekerasan Permukaan Titanium dengan Variasi Waktu 20, 40, 60, 80 Menit. Skripsi thesis, Universitas Muhammadiyah Surakarta.
PDF (NASKAH PUBLIKASI)
NASKAH PUBLIKASI.pdf Download (1MB) |
|
PDF (HALAMAN DEPAN)
HALAMAN DEPAN.pdf Download (880kB) |
|
PDF (BAB I)
BAB I.pdf Download (145kB) |
|
PDF (BAB II)
BAB II.pdf Restricted to Repository staff only Download (556kB) | Request a copy |
|
PDF (BAB III)
BAB III.pdf Restricted to Repository staff only Download (805kB) | Request a copy |
|
PDF (BAB IV)
BAB IV.pdf Restricted to Repository staff only Download (724kB) | Request a copy |
|
PDF (BAB V)
BAB V.pdf Restricted to Repository staff only Download (127kB) | Request a copy |
|
PDF (DAFTAR PUSTAKA)
DAFTAR PUSTAKA.pdf Download (110kB) |
|
PDF (LAMPIRAN)
LAMPIRAN.pdf Restricted to Repository staff only Download (3MB) | Request a copy |
|
PDF (PERNYATAAN TIDAK PUBLIKASI)
PERNYATAAN TIDAK PUBLIKASI.pdf Restricted to Repository staff only Download (374kB) | Request a copy |
Abstract
the research was conducted to develop the surface hardness of titanium by nickel electroplating method. it is hopes that this method will be more effective in term of cost and production process. the purpose of the research is into to find out the surface hardness of titanium after electroplating nickel. in this research, the method use testing process is coating thickness, roughness test, and surface hardness test. the basic material used titanium plate with thickness 3 mm and coating material is nickel with electroplating method with variation of spraying time 20 minutes, 40 minutes, 60 minutes, 80 minutes at 2,8 volt.base on the research has been done, the authors have obtained the test result. the nickel electroplating process at the variation of dyeing time at 2,8 volt was found that the highest coating thickness level of 36,34 µm, the lowest roughness level occurred at 80 minutes dyeing that was 0,211 µm, highest surface hardness of 571,42 HV, compare to the material before electroplating was 173,88 HV.
Item Type: | Karya ilmiah (Skripsi) |
---|---|
Uncontrolled Keywords: | Titanium, Elektroplating, Ketebalan Lapisan, Kekasaran Permukaan dan Kekekerasan Permukaan |
Subjects: | T Technology > TP Chemical technology |
Divisions: | Fakultas Teknik > Teknik Mesin |
Depositing User: | DANANG DANY YANTO |
Date Deposited: | 17 Jul 2018 04:14 |
Last Modified: | 17 Jul 2018 04:14 |
URI: | http://eprints.ums.ac.id/id/eprint/63459 |
Actions (login required)
View Item |