Analisis X-Ray Diffraction (XRD) Pada Friction Stir Welding Pada Aluminium Seri 6061-T6 Dengan Penambahan Filler Pelat Seng Dan Pelat Kuningan

Aji, Yogi Bawono and -, Agus Dwi Anggono, ST, M.Eng, Ph.D (2020) Analisis X-Ray Diffraction (XRD) Pada Friction Stir Welding Pada Aluminium Seri 6061-T6 Dengan Penambahan Filler Pelat Seng Dan Pelat Kuningan. Skripsi thesis, Universitas Muhammadiyah Surakarta.

[img] PDF (Naskah Publikasi)
yogi Naskah Publikasi-27.pdf

Download (855kB)
[img] PDF (Halaman Depan)
yogi Halaman Awal-1.pdf

Download (800kB)
[img] PDF (Bab I)
BAB 1.pdf

Download (311kB)
[img] PDF (Bab II)
BAB II.pdf
Restricted to Repository staff only

Download (1MB) | Request a copy
[img] PDF (Bab III)
BAB III.pdf
Restricted to Repository staff only

Download (466kB) | Request a copy
[img] PDF (Bab IV)
BAB IV.pdf
Restricted to Repository staff only

Download (524kB) | Request a copy
[img] PDF (Bab V)
BAB V.pdf
Restricted to Repository staff only

Download (304kB) | Request a copy
[img] PDF (Daftar Pustaka)
Daftar Pustaka.pdf

Download (355kB)
[img] PDF (Lampiran)
Lampiran.pdf
Restricted to Repository staff only

Download (623kB) | Request a copy
[img] PDF (Surat Pernyataan Publikasi)
surat pernyataan publikasi.pdf
Restricted to Repository staff only

Download (249kB) | Request a copy

Abstract

The purpose of this study was to study the differences in crystal structure and composition characteristics of the welding results by the Friction Stir Welding (FSW) method through X-ray diffraction (XRD) testing. The material used in this research is aluminum alloy 6061-T6 series. In this process, fillers are used from brass plates and zinc plates. Therefore, variations of the specimen are FSW with filler and without filler. The results of the study showed the Crystal Structure Characteristics of each material, the first material formed was not Aluminium, the highest peak was obtained at an angle of 38.52 ° with an intensity of 9224 Cps, the crystal structure was Face Center Cubic with a lattice length of 52.86 nm and a density of 2.717 g/cm3 , the second material is formed Al2 O4 Zn Compound, the highest peak can be obtained at an angle 783.16 ° with an intensity of 760 Cps, Hexagon shaped crystal structure with a lattice length of 65.6 nm and a density of 4.724 g/cm3 , the material produced by the Compound Cu Zn, The highest peak can be obtained at an angle of 38.54 ° with an intensity of 3458 Cps. The crystalline structure forms a Face Center Cubic with a lattice length of 0 nm and a density of 8.338 g/cm3 , and the composition of Al2 Cu, the highest peak can be at an angle of 78.24 ° with intensity 1094, the crystal structure is Tetragonal with a lattice length of 109.2 nm and a density of 4,348 g/cm3

Item Type: Karya ilmiah (Skripsi)
Uncontrolled Keywords: Friction Friction Welding, X-Ray Diffraction, Crystal Structure, Aluminum.
Subjects: T Technology > TJ Mechanical engineering and machinery
Divisions: Fakultas Teknik > Teknik Mesin
Depositing User: YOGI BAWONO AJI
Date Deposited: 21 Feb 2020 09:22
Last Modified: 21 Feb 2020 09:22
URI: http://eprints.ums.ac.id/id/eprint/81558

Actions (login required)