, Gunanto and , Ir. Aliem Sudjatmiko, M.T. (2019) Peninjauan Kuat Tekan, Kuat Tarik dan Kuat Lentur Batako dengan Menambahkan Limbah Pecahan Genteng pada Campuran Batako. Skripsi thesis, Universitas Muhammadiyah Surakarta.
PDF (Naskah Publikasi)
NASKAH PUBLIKASI-10.pdf Download (480kB) |
|
PDF (Halaman Depan)
HALAMAN DEPAN GUNANTO.pdf Download (593kB) |
|
PDF (Bab I)
BAB I.pdf Download (448kB) |
|
PDF (Bab II)
BAB II.pdf Restricted to Repository staff only Download (448kB) | Request a copy |
|
PDF (Bab III)
BAB III.pdf Restricted to Repository staff only Download (448kB) | Request a copy |
|
PDF (Bab IV)
BAB IV.pdf Restricted to Repository staff only Download (546kB) | Request a copy |
|
PDF (Bab V)
BAB V.pdf Restricted to Repository staff only Download (168kB) | Request a copy |
|
PDF (Bab VI)
BAB VI.pdf Restricted to Repository staff only Download (12kB) | Request a copy |
|
PDF (Daftar Pustaka)
DAFTAR PUSTAKA.pdf Download (12kB) |
|
PDF (Lampiran)
LAMPIRAN.pdf Restricted to Repository staff only Download (1MB) | Request a copy |
|
PDF (Surat Pernyataan Publikasi)
SURAT PERNYATAAN.pdf Restricted to Repository staff only Download (469kB) | Request a copy |
Abstract
Hollow concrete or lightweight concrete is concrete whose aggregate is replaced by lightweight aggregate such as fine aggregate, cement, water with a certain ratio. Hollow brick is one of the lightweight concrete molds that is often used in making walls, because concrete brick is more practical and more time efficient. Batako in this research was developed with the addition of a mixture, among others, by adding tile fragments. The purpose of this study is to find out how much influence the roof tile additives have in making concrete blocks by testing the compressive strength, flexural strength, and tensile strength. This research uses specimen in the form of brick with a size of 30 x 15 x 10 cm for the flexural strength test of the brick, beam size of 10 x 10 cm for the brick compressive strength test. I later brick mold with a middle size of mold 10 x 10 cm. The number of specimens made in this study were 45 specimens and for the comparison of the volume of fine aggregate and cement was 1: 6. The cement water factor used was 0.35. The added ingredients used are 0%, 5% and 10%, of the volume of sand. The specimens were left in normal humid air for 28 days and then tested the specimens including compressive strength, flexural and pure tensile tests. Based on the research, it was found that the best compressive strength was 5.40 MPa with the proportion of addition of broken tile 0%. with the proportion of additional 10% tile shards.
Item Type: | Karya ilmiah (Skripsi) |
---|---|
Uncontrolled Keywords: | tensile strength, concrete brick, compressive strength, flexural strength, tileshards |
Subjects: | T Technology > TA Engineering (General). Civil engineering (General) |
Divisions: | Fakultas Teknik > Teknik Sipil |
Depositing User: | GUNANTO |
Date Deposited: | 14 Sep 2019 04:46 |
Last Modified: | 14 Sep 2019 04:46 |
URI: | http://eprints.ums.ac.id/id/eprint/77728 |
Actions (login required)
View Item |