Santoso, Ibrahim Aji Eko Imam and , Bambang Waluyo F, ST. MT (2018) Pengaruh Asam Klorida (HCl) Terhadap Terak Alumunium Pada Pembuatan Batu Gerinda. Diploma thesis, Universitas Muhammadiyah Surakarta.
PDF (Naskah Publikasi)
NASKAH PUBLIKASI.pdf Download (2MB) |
|
PDF (Halaman Depan)
halaman depan.pdf Download (1MB) |
|
PDF (Bab I)
BAB I ibra.pdf Download (157kB) |
|
PDF (Bab II)
BAB II ibra.pdf Restricted to Repository staff only Download (605kB) |
|
PDF (Bab III)
BAB III ibra.pdf Restricted to Repository staff only Download (807kB) |
|
PDF (Bab IV)
BAB IV ibra.pdf Restricted to Repository staff only Download (422kB) |
|
PDF (Bab V)
BAB V ibra.pdf Restricted to Repository staff only Download (88kB) |
|
PDF (Daftar Pustaka)
DAFTAR PUSTAKA.pdf Download (13kB) |
|
PDF (Lampiran)
LAMPIRAN.pdf Restricted to Repository staff only Download (1MB) |
|
PDF (Surat Pernyataan Publikasi Ilmiah)
surat pernyataan artikel publikasi.pdf Restricted to Repository staff only Download (488kB) |
Abstract
Grinding is a tool used for the process of reducing and cutting an abrasive workpiece through friction between the abrasive material and the workpiece. In addition, the grinding process can also for the process of finishing workpieces (refine the workpiece surface) smoothed the pieces, welding results,can also as a metal sharpener such as knives and chisels. In this research, the manufacture of self-assembled grinding wheels with aluminum slag materials that have been washed as abrasion material that aims to find out how much the rate of wear and grind own specimen grinding wheels, previous research, and the existing grinding wheels in the market market with Lippro brand. The process of making grinding wheels begins with the preparation of materials to be used, namely liquid phenolic resins and powders, slag cast aluminum, mesh 12 and 40 that have been treated with water and HCl, and fiberglass mesh fiber. After that mix all the ingredients according to the composition that has been determined. Furthermore all materials are inserted in the mold and compressed with a press machine with a 15 ton force for 5 minutes. Then ignored at room temperature of at least 24 hours.Then sintered with temperature 1400C for 1 hour. Tests performed are wear test with ASTM D-3702 standard. From the results of research shows that the wear value of Lippro brand grinding wheel has a low wear rate compared to homemade grinding stone.
Item Type: | Karya ilmiah (Diploma) |
---|---|
Uncontrolled Keywords: | grinding stone, phenolic resin, aluminum slag, HCl |
Subjects: | T Technology > TJ Mechanical engineering and machinery |
Divisions: | Fakultas Teknik > Teknik Mesin |
Depositing User: | IBRAHIM AJI EKO IMAM SANTOSO |
Date Deposited: | 07 Feb 2018 09:29 |
Last Modified: | 07 Feb 2018 09:30 |
URI: | http://eprints.ums.ac.id/id/eprint/59583 |
Actions (login required)
View Item |