Nugroho, Sahrul Apri and , Ir. Aliem Sudjatmiko, M.T. (2017) Tinjauan Kekuatan Beton dengan Bahan Dasar Pasir dan Kerikil Trengguli dari Jenawi Karanganyar Sebagai Bahan Agregat Halus dan Kasar. Diploma thesis, Universitas Muhammadiyah Surakarta.
PDF (Naskah Publikasi)
Naskah Publikasi-194.pdf Download (1MB) |
|
PDF (Halaman Depan)
HALAMAN DEPAN.pdf Download (1MB) |
|
PDF (BAB I)
BAB 1 SAHRUL AN.pdf Download (165kB) |
|
PDF (BAB II)
BAB 2 SAHRUL AN.pdf Restricted to Repository staff only Download (308kB) | Request a copy |
|
PDF (BAB III)
BAB 3 SAHRUL AN.pdf Restricted to Repository staff only Download (300kB) | Request a copy |
|
PDF (BAB IV)
BAB 4 SAHRUL AN.pdf Restricted to Repository staff only Download (1MB) | Request a copy |
|
PDF (BAB V)
BAB 5 SAHRUL AN.pdf Restricted to Repository staff only Download (349kB) | Request a copy |
|
PDF (BAB VI)
BAB 6 SAHRUL AN.pdf Restricted to Repository staff only Download (93kB) | Request a copy |
|
PDF (Daftar Pustaka)
DAFTAR PUSTAKA.pdf Download (184kB) |
|
PDF (Lampiran)
LAMPIRAN.pdf Restricted to Repository staff only Download (2MB) | Request a copy |
|
PDF (Surat Pernyataan)
SURAT PERNYATAAN PUBLIKASI KARYA ILMIAH.pdf Restricted to Repository staff only Download (187kB) | Request a copy |
Abstract
Concrete is a mixture of cement, coarse aggregate, fine aggregate and water. Sometimes wear materials that vary greatly, ranging from chemicals plus materials, fiber to non-chemical building materials at a certain percentage. In this research to know strength of compressive strength and tensile strength of concrete use of local aggregate that is sand and gravel of Trengguli from Jenawi Karanganyar. This study also finds out the strength difference with aggregate as it is in the field and aggregate after washing. The number of specimens for each aggregate variation is, after washing and for normal concrete with a fase of 0.4 and 0.5 of 3 pieces, so that the total number of specimens is 36. The test specimens used are cylindrical in diameter 15 cm and 30 cm high. On the test results of compressive strength and maximum tensile strength obtained on aggregate variation after washing with fas 0,4. Aggregate as it is, yields a compressive strength of 19.81 MPa at 0.4 and 2.00 MPa fas on 0.4 for tensile strength. Aggregate after washing yields a compressive strength of 21.51 MPa on a fase of 0.4 and for tensile strength of 2.25 MPa at 0.4 phases. While for normal concrete the resultant strength of 25,47 MPa pressed on fas 0,4 and tensile strength equal to 2,97 MPa at fas 0,4.
Item Type: | Karya ilmiah (Diploma) |
---|---|
Uncontrolled Keywords: | Aggregate care, concrete, local aggregates, water cement factors |
Subjects: | T Technology > TA Engineering (General). Civil engineering (General) |
Divisions: | Fakultas Teknik > Teknik Sipil |
Depositing User: | SAHRUL APRI NUGROHO |
Date Deposited: | 27 Dec 2017 03:54 |
Last Modified: | 27 Dec 2017 03:54 |
URI: | http://eprints.ums.ac.id/id/eprint/57816 |
Actions (login required)
View Item |