Kristiyanto, Kristiyanto and , Wijianto, ST. MEng. Sc. and , Ir. Bibit Sugito, MT (2016) Analisis Komposit Dengan Penguat Serat Nanas 40% Dan Serbuk Kayu Sengon 60% Pada Fraksi Volume 40%,50%,60% Bermatrik Resin Polyester Untuk Panel Akuistik. Diploma thesis, Universitas Muhammadiyah Surakarta.
PDF (HALAMAN DEPAN)
HALAMAN JUDUL.pdf Download (1MB) |
|
PDF (BAB I)
BAB I.pdf Download (111kB) |
|
PDF (BAB II)
BAB II.pdf Restricted to Repository staff only Download (589kB) | Request a copy |
|
PDF (BAB III)
BAB III.pdf Restricted to Repository staff only Download (734kB) | Request a copy |
|
PDF (BAB IV)
BAB IV.pdf Restricted to Repository staff only Download (737kB) | Request a copy |
|
PDF (BAB V)
BAB V.pdf Restricted to Repository staff only Download (196kB) | Request a copy |
|
PDF (DAFTAR PUSTAKA)
DAFTAR PUSTAKA.pdf Download (190kB) |
|
PDF (LAMPIRAN)
LAMPIRAN.pdf Restricted to Repository staff only Download (6MB) | Request a copy |
|
PDF (SURAT PERNYATAAN PUBLIKASI)
PERNYATAAN PUBLIKASI.pdf Restricted to Repository staff only Download (427kB) | Request a copy |
|
PDF (Naskah Publikasi)
NASKAH PUBLIKASI_kris1.pdf Download (1MB) |
Abstract
Purpose of the research is to know tensile strength, bending and acoustic impedance of pineapple fiber composite at volume fraction of (40%, 50%, and 60%). The composite is made by using mold press method. The composite is made from pineapple fiber and sengon sawdust with polyester resin of Yukalac 157 BQTN – EX and MEKPO catalyst, and volume fraction variation of 40%, 50%, 60%. Press mold was used to make the composite. The composite was tested according to ASTM D 638-02 standard. ASTM D790-02 for tensile strength and ANSI S1-13 for acoustic impedance test. Results of the research indicated that average tensile strength at volume fraction of 60% was 34.680 MPa and lowest result at fraction of 40% was 27.189 MPa. The highest averaged elasticity modulus was found at volume fraction of 60%, namely 46.240 MPa and, the lowest one was at fraction volume of 40%, namely 45.315 MPa. Results of tensile strength testing were: the highest averaged tensile strength of 57.504 MPa was found at fraction of 60% and the lowest one of 39.166 MPa was found at fraction of 40%. Results of acoustic impedance with spon were: the highest results were found at volume fraction of 50%, namely 62.06 dB and the lowest one was found at fraction of 60%, namely 61.89 dB. Then, results without spon found the highest at fraction of 50%, 62.07 dB and the lowest was found at fraction of 40%, 61.81 dB Key words: Tensile strength, bending test, acoustic impedance
Item Type: | Karya ilmiah (Diploma) |
---|---|
Uncontrolled Keywords: | Uji Tarik, Uji Bending, Impedansi Akuistik |
Subjects: | Q Science > Q Science (General) |
Divisions: | Fakultas Teknik > Teknik Mesin |
Depositing User: | KRISTIYANTO |
Date Deposited: | 09 Aug 2016 03:35 |
Last Modified: | 09 Aug 2016 03:35 |
URI: | http://eprints.ums.ac.id/id/eprint/45215 |
Actions (login required)
View Item |