Irsyad, Mirwan and , Ir. Ngafwan, MT. and , Agus Yulianto, ST. MT. (2015) Sifat Fisis Dan Mekanis Pada Komposit Polyester Serat Batang Pisang Yang Disusun Asimetri [ 45o / -30o / 45o / -30o ]. Diploma thesis, Universitas Muhammadiyah Surakarta.
PDF (Naskah Publikasi)
NASKAH PUBLIKASI.pdf Download (1MB) |
|
PDF (Halaman Depan)
HALAMAN DEPAN.pdf Download (693kB) |
|
PDF (Bab I)
BAB I.pdf Download (98kB) |
|
PDF (Bab II)
BAB II.pdf Restricted to Repository staff only Download (717kB) |
|
PDF (Bab III)
BAB III.pdf Restricted to Repository staff only Download (703kB) |
|
PDF (Bab IV)
BAB IV.pdf Restricted to Repository staff only Download (2MB) |
|
PDF (Bab V)
BAB V.pdf Restricted to Repository staff only Download (87kB) |
|
PDF (Daftar Pustaka)
DAFTAR PUSTAKA.pdf Download (126kB) |
|
PDF (Lampiran)
LAMPIRAN.pdf Restricted to Repository staff only Download (15MB) |
|
PDF (Pernyataan Publikasi Ilmiah)
PERNYATAAN PUBLIKASI.pdf Restricted to Repository staff only Download (587kB) |
Abstract
The aim of this study was to describe the tensile strength, bending strength and fracture macro photo on banana stem fiber polyester composites prepared asymmetry [45o / -30o / 45o / -30o] to change teperature test on tensile test and bending test. The initial process of making composites are making fibers from banana trees followed by immersion for 2 hours using a chemical solution of kalium pemangante (KMnO4) by 2% per 1 liter of distilled water. Drying under the sun to dry continued with the process of oven for 1 hour at a constant temperature of 35oC until the moisture content of 10%. Then the fibers are arranged at an angle of orientation of asymmetry [45o / -30o / 45o / -30o] using paper prints, be continued with the provision of the resin was conducted using hand lay-up on the glass mold that has been measured in accordance with the standards. The resin used is a thermosetting resin types, namely polyester BQTN series 157 with increasing catalyst (hardener) as much as 1% of the volume of resin. Tensile test using the ASTM D 3039 standard while bending tests using standard ASTM D 7264 with a variation of room temperature, test temperature of 35oC, 45oC and 55oC. Results of tensile test can be concluded that the tensile strength at room temperature is 11.530 N / mm2, the temperature variation of the tensile test, the greater the given temperature tensile strength will increasingly come down from 15.520 N / mm2 at a temperature test 35oC be 9.502 N / mm2 at temperatures 55oC test. While the test results of bending can be concluded that the bending strength at room temperature is 0.151 N / mm2, the temperature variation of bending test, the higher the temperature of a given strength of bending will experience kenakian of 0,339 N / mm2 at a temperature test 35oC be 6.215 N / mm2 at temperatures test 55oC.
Item Type: | Karya ilmiah (Diploma) |
---|---|
Uncontrolled Keywords: | Komposit Polyester, Susunan Asimetri, Serat batang pisang |
Subjects: | T Technology > TJ Mechanical engineering and machinery |
Divisions: | Fakultas Teknik > Teknik Mesin |
Depositing User: | Mirwan Irsyad |
Date Deposited: | 06 Oct 2015 06:12 |
Last Modified: | 13 Oct 2021 01:55 |
URI: | http://eprints.ums.ac.id/id/eprint/37615 |