Subekti, Wildan Arya Nanda and , Ir. Agung Setyo Darmawan, S.T., M.T., IPM. (2023) Pengaruh Anil pada Suhu 850oC dengan Waktu Tahan 20 Menit terhadap Struktur Mikro dan Kekerasan Brinell Besi Cor Putih. Skripsi thesis, Universitas Muhammadiyah Surakarta.
PDF (Naskah Publikasi)
NASKAH PUBLIKASI.pdf Download (916kB) |
|
PDF (Halaman Depan)
HALAMAN DEPAN.pdf Download (1MB) |
|
PDF (Bab I)
BAB I.pdf Download (188kB) |
|
PDF (Bab II)
BAB II.pdf Restricted to Repository staff only Download (1MB) | Request a copy |
|
PDF (Bab III)
BAB III.pdf Restricted to Repository staff only Download (910kB) | Request a copy |
|
PDF (Bab IV)
BAB IV.pdf Restricted to Repository staff only Download (1MB) | Request a copy |
|
PDF (Bab V)
BAB V.pdf Restricted to Repository staff only Download (59kB) | Request a copy |
|
PDF (Daftar Pustaka)
DAFTAR PUSTAKA.pdf Download (97kB) |
|
PDF (Lampiran)
LAMPIRAN.pdf Restricted to Repository staff only Download (1MB) | Request a copy |
|
PDF (Surat Pernyataan Publikasi)
Surat Pernyataan Publikasi.pdf Restricted to Repository staff only Download (246kB) | Request a copy |
Abstract
In the world of the metal casting industry, we often hear about a type of cast iron called white cast iron. White cast iron is a type of cast iron that does not have graphite so it has mechanical properties that are very hard but brittle. This research aims to determine the effect of annealing at a temperature of 850°C with a holding time of 20 minutes on the microstructure, phase chemical composition, and hardness value of white cast iron. Metallographic testing and composition testing were carried out using Scanning Electron Microscope – Energy Dispersive X-Ray Spectroscopy (SEM-EDS), while hardness testing was carried out using the Brinell method. The results of SEM-EDS testing show that white cast iron that has undergone an annealing process contains graphite, cementite (Fe3C) and pearlite phases. In the graphite phase there are Carbon (C) elements of 79.88% by weight, Ferro (Fe) by 16.11% by weight, and Oxygen (O) by 4% by weight. Then in the cementite phase (Fe3C) there are Ferro elements (Fe) amounting to 92.60% by weight, Carbon (C) by 7.30% by weight, and Oxygen (O) by 0.10% by weight. And in the pearlite phase there are Ferro (Fe) elements of 86.31% by weight, Silicon (Si) by 4.49%, Carbon (C) by 3.59% by weight, Aluminum (Al) by 1.09% by weight, and Oxygen (O) element is 4.49% by weight. The results of hardness testing show that the highest hardness value occurs in raw material with an average hardness value of 474.163 BHN. Meanwhile, the lowest hardness value occurred in test specimens that had been annealed with an average hardness value of 379,497 BHN.
Item Type: | Thesis (Skripsi) |
---|---|
Uncontrolled Keywords: | Besi cor putih, struktur mikro, kekerasan brinell, anil |
Subjects: | T Technology > TJ Mechanical engineering and machinery T Technology > TS Manufactures |
Divisions: | Fakultas Teknik > Teknik Mesin |
Depositing User: | WILDAN ARYA NANDA SUBEKTI |
Date Deposited: | 19 Dec 2023 01:45 |
Last Modified: | 19 Dec 2023 01:45 |
URI: | http://eprints.ums.ac.id/id/eprint/119088 |
Actions (login required)
View Item |