Saputra, Roman Rio and , Agung Setyo Darmawan, ST. MT (2020) Analisa Permukaan Patahan Spesimen Uji Impak Besi Cor Nodular Dengan Variasi Kandungan Magnesium 0,0296%, 0,0307% Dan 0,0336%. Skripsi thesis, Universitas Muhammadiyah Surakarta.
PDF (Naskah Publikasi)
naskah baru.pdf Download (868kB) |
|
PDF (Halaman Depan)
HALAMAN DEPAN.pdf Download (736kB) |
|
PDF (Bab I)
BAB I.pdf Download (165kB) |
|
PDF (Bab II)
BAB II.pdf Restricted to Repository staff only Download (642kB) | Request a copy |
|
PDF (Bab III)
BAB III.pdf Restricted to Repository staff only Download (614kB) | Request a copy |
|
PDF (Bab IV)
BAB IV.pdf Restricted to Repository staff only Download (743kB) | Request a copy |
|
PDF (Bab V)
BAB V.pdf Restricted to Repository staff only Download (91kB) | Request a copy |
|
PDF (Daftar Pustaka)
DAFTAR PUSTAKA.pdf Download (157kB) |
|
PDF (Lampiran)
LAMPIRAN.pdf Restricted to Repository staff only Download (588kB) | Request a copy |
|
PDF (Surat Pernyataan Publikasi)
SURAT PERNYATAAN PUBLIKASI baru.PDF Restricted to Repository staff only Download (105kB) | Request a copy |
Abstract
This study aims to determine the effect of variations in the content of magnesium (Mg) nodular cast iron on the microstructure and fracture surface of nodular cast iron impact test specimens.This research uses FCD (ferro casting ductile) as a starting material which is then melted in a melting furnace. The process of forming round graphite cast iron is carried out using an open ladel system, namely the variation of the addition of FeSiMg 0 grams (raw material), 50 grams and 100 grams which is placed at the bottom of the ladle with a capacity of 15 kg just before the molten iron is poured into the ladle.The results showed that the more magnesium (Mg) content, the resulting graphite grains tended to decrease and tend to shrink, more pearlite and less ferrite. Meanwhile, from SEM testing that each specimen has a mixed fracture, namely clay and brittle fractures. The fracture surface shows the more magnesium content the more brittle fracture areas are according to Kartika's research (2019). However, specimen 3 appears to have more clay fracture areas, this is due to the uneven mixing of FeSiMg.
Item Type: | Karya ilmiah (Skripsi) |
---|---|
Uncontrolled Keywords: | Nodular iron, micro photo and SEM |
Subjects: | T Technology > TJ Mechanical engineering and machinery |
Divisions: | Fakultas Teknik > Teknik Mesin |
Depositing User: | ROMAN RIO SAPUTRA |
Date Deposited: | 16 Sep 2020 03:14 |
Last Modified: | 16 Sep 2020 03:14 |
URI: | http://eprints.ums.ac.id/id/eprint/85965 |
Actions (login required)
View Item |