Pengaruh PHR Ijuk terhadap Sifat Fisis dan Mekanis Material Ijuk Karet

Amirrudin, Nanang and , Masyrukan, ST, MT (2017) Pengaruh PHR Ijuk terhadap Sifat Fisis dan Mekanis Material Ijuk Karet. Diploma thesis, Universitas Muhammadiyah Surakarta.

[img] PDF (Naskah Publikasi)
NASKAH PUBLIKASI-116.pdf

Download (1MB)
[img] PDF (Halaman Depan)
HALAMAN DEPAN.pdf

Download (1MB)
[img] PDF (BAB I)
BAB I.pdf

Download (119kB)
[img] PDF (BAB II)
BAB II.pdf
Restricted to Repository staff only

Download (438kB)
[img] PDF (BAB III)
BAB III.pdf
Restricted to Repository staff only

Download (1MB)
[img] PDF (BAB IV)
BAB IV.pdf
Restricted to Repository staff only

Download (380kB)
[img] PDF (BAB V)
BAB V.pdf
Restricted to Repository staff only

Download (99kB)
[img] PDF (DAFTAR PUSTAKA)
DAFTAR PUSTAKA.pdf

Download (112kB)
[img] PDF (LAMPIRAN)
LAMPIRAN.pdf
Restricted to Repository staff only

Download (12MB)
[img] PDF (surat pernyataan artikel publikasi)
SURAT PERNYATAAN ARTIKEL PUBLIKASI.pdf
Restricted to Repository staff only

Download (175kB)

Abstract

The aim of this study is to know the elements in the specimen by doing x-ray testing. And to find out how strong the specimens are made with tear and tear testing process. With variation Composition of fibers particles 8 phr, 13 phr, 18 phr. This research uses latex as a matrix and powder as a mixture material. The process begins with the washing, soaking and drying of the fibers and then the preparation of the powder,then mix the latex with the powder of the fibers in the mixing container and stir until mixed evenly and then pour into the mold for the vulcanization process, after which make the specimen for testing, then the specimen is tested According to XRF x-ray testing standards,tear testing with ISO 34-1: 2015 and tensile testing with SNI ISO 37: 2015 (IDT-2011). In the X-Ray ray test, we found three elements of metal content (Zn, Fe and Ti). The highest content of Zn metal in the powdered fibers with a content of 8 phr of 3.46%, for the highest.Fe content of fibers fibers with 18 phr content of 1.036 %, And the highest Ti content in fibers fibers with a content of 18 phr of 0.809%. In the tensile test results that have been done can be concluded that the highest tensile stress is obtained on the compound with the content of 8 phr powder fibers with a tensile stress value of 10.56 N

Item Type: Karya ilmiah (Diploma)
Uncontrolled Keywords: Keywords: latex, fibers, dispersion, vulcanization
Subjects: T Technology > TA Engineering (General). Civil engineering (General)
Divisions: Fakultas Teknik > Teknik Mesin
Depositing User: NANANG AMIRRUDIN
Date Deposited: 03 Oct 2017 08:12
Last Modified: 03 Oct 2017 08:13
URI: http://eprints.ums.ac.id/id/eprint/56074

Actions (login required)

View Item View Item